Lithium battery positive electrode material project case study
Material: NCM sintered crushed material.
Bulk density of materials: 1-1.8 kg/cm ³。
Conveying output: 550Kg/h.
Conveying distance: 190 meters.
Design calculation
Delivery tank capacity: 140L.
Effective diameter of conveying pipeline: 3 inches.
Average gas consumption: 1.65m ³/ Min.
Compressed gas supply flow rate: 2.96 m ³/ Min.
Compressed gas storage tank size: 900L.